Common Plastic Injection Molding Defects and How to Fix Them


In any stage of the manufacturing process, you can run into defects. Sometimes, it comes from inexperience or machinery issues

BriefingWire.com, 9/30/2016 - It might just happen from time to time. It’s important to remember defects happen to even the best. An experienced technician can recognize and correct these defects, though. In some cases, they can minimize or even eliminate the occurrence altogether.

The most common plastic injection molding defects don’t necessarily come from the operator. They’re related to three things: the resin, the injection molding process, or the molding.

Resin and Additive-Related Defects

There are two common defects you might see related to resin and additives. The first is delamination. You should never see this in a finished product, but a technician might notice flakiness around the surface. This isn’t just an aesthetic problem. It can also reduce the strength. This happens when the resin pellets have been contaminated by moisture or a dissimilar resin. It can also be caused by release agents in the molding.

Plastic injection molding services often prevent this problem with simple solutions. For example, they can pre-dry the resin pellets or increase the temperature of the mold. When mold release agents cause delamination, companies use a mold redesign with more focus on the ejection mechanism. When dissimilar resins are mixed, the only solution is to replace the resin.

The second common issue associated with the resins is discoloration. In other words, part or all of the color isn’t what it was expected to be. This is often an easy fix. Clearing leftover pellets out of the hopper can resolve the problem. Experts also check the barrel temperature. Technicians can flush the hopper and feed zone between processes. This way, they automatically resolve the problem.

Process-Related Molding Defects

Even with many advancements in technology, we still see process-related defects in injection molding. We sometimes run into burn marks, which are exactly what they sound like: surface marks. Depending on the severity, it can cause degraded plastics. Air gets trapped causing overheated resin. How can you avoid burn marks? You can decrease the resin injection speeds. This reduces the risk of trapped air. You can also use venting and degassing systems to achieve the same effect. Finally, you can reduce the mold and melt temperature.

Second, you might see flow marks, which are typically wavy or lined areas. It can also show up as discoloration on the part surface. This happens when the resin cools too quickly or when there’s an improper gate location. The solution for this plastic injection molding defect is as simple as increasing the injection speed and pressure. This helps to control the filling and cooling. Sometimes, this isn’t enough, though. In these cases, you’ll need to redesign the mold to avoid sudden flow direction changes.

================================

Plastimold

250 N Congress Ave

Delray Beach, FL, 33445

Phone: 561-869-0183

sales@plastimoldproducts.com

http://www.plastimoldproducts.com

 
 
FAQs | Contact Us | Terms & Conditions | Privacy Policy
© 2026 Proserve Technology, Inc.