First, we should know 3PE coating steel grinding reserved section at the polyethylene layer groove, the pipe end weld reinforcement is not grinding or grinding uneven, will result in the weld epoxy powder protruding portion is polyethylene bottom Under worn in open dumps for a long time anti-corrosion pipe case, the weld surface of the metal will be corroded, causing the phenomenon 3PE coating edge lifting.Measures to avoid edge lifting 3PE coating pipe end appears is:
1. Without prejudice to the case of welding nozzles, should be increased polyethylene layer ends epoxy powder reserve length, can prevent a long time because of steel piling pipe end metal corrosion caused serious 3PE anticorrosion Alice.
2, anti-corrosion pipe open dumps for a long time, should be covered in the pipe end to prevent water erosion, causing severe corrosion pipe end.
3, if the pipeline construction site longer period, in the tube at the end of the metal exposed brushing weldable rust to prevent pipe corrosion caused by corrosion during storage 3PE coating Alice.
4, strict control of pipe weld reinforcement at the end of the reserve grinding quality. Like in the weld polyethylene tube slope estuary and other parts of the epoxy powder retention length> 20mm, in order to prevent the bottom of the weld corrosion epoxy powder is first caused 3PE coating Alice.
5, sections reserved only to protect the integrity epoxy powder coating, in order to play Alice pipe end delay caused by corrosion. Domestic polyethylene pipe end beveling are polished manner with a wire wheel, it will damage the epoxy powder coating. Should be replaced by machining grooves, the bottom edge to limited means to control infeed bit depth of the tool, to avoid harming the epoxy powder coating.